Monel® 400

A Nickel-Copper alloy with high strength and excellent corrosion resistance in a range of acidic and alkaline environments and suitable for reducing conditions. It also has good ductility and thermal conductivity. Used in a variety of applications, Monel® 400 has excellent resistance to seawater, and can also be used in hydrochloric and hydrofluoric acids.

Monel® 400 is also known as Phyweld 400 and Nicorros LC.

Available in all profile options

Monel® 400 - Alloy Wire International 1

Key Features

Monel® 400 offers the following key features:

Excellent corrosion resistance in a wide range of acidic & alkaline environments
Especially suitable for reducing conditions
Good ductility & thermal conductivity
Good for sea water applications

Typical Applications

Monel® 400 is known to be suitable for the following applications:

Marine engineering
Chemical processing
Hydro-carbon processing
Heat exchangers
Valves
Pumps


Designations

W.Nr 2.4361
W.Nr 2.4360
UNS N04400
AWS 040

Specifications

AMS 4730
ASTM B164
BS 3075 NA 13
BS 3076 NA 13
DTD 204B
ISO 15156-3
(NACE MR 0175)
QQ-N-281

Chemical Composition

The chemical composition of Monel® 400 is indicated in the table below:

ElementMin %Max %
C0.3
Si0.50
Mn2.00
S0.024
Cu28.0034.00
Fe2.50
Ni+Co63.0070.00
Co2.0

Alloy Details

Monel® 400 density, melting point, coefficient of expansion, modulus of rigidity, and elasticity is indicated in the table below:

DensityMelting PointCoefficient of ExpansionModulus of RigidityModulus of Elasticity
8.8 g/cm³1350 °C13.9 μm/m °C (20 – 100 °C)65.3 kN/mm²173 kN/mm²
0.318 lb/in³2460 °F7.7 x 10-6 in/in °F (70 – 212 °F)9471 ksi25092 ksi

Heat treatment of finished parts

The typical heat treatment of Monel® 400:

Condition as supplied by AWITypeTemperatureTimeCooling
Annealed or Spring TemperStress Relieve300 – 320 °C
(570 – 610 °F)
0.5 – 1 HrAir

Properties

The typical mechanical properties of Monel® 400:

Annealed
Approx. tensile strength<600 N/mm²<87 ksi
Approx. operating temperature-200 to +230 °C-330 to +445 °F
Spring Temper
Approx. tensile strength800 – 1100 N/mm²116 – 160 ksi
Approx. operating temperature-200 to +230 °C-330 to +445 °F

The above tensile strength ranges are typical. If you require different please ask.