These hot cutting wires have high strength at elevated temperatures and are used for cutting foam polystyrene (EPS) and or heat sealing woven polypropylene bags.
To achieve the best cut, adjust the temperature and cutting speed. The material type and it's density will influence the cutting speed.
| RW 118 Properties | ||
| DENSITY | 8.18 g/cm3 | |
| ELECTRICAL RESISTIVITY AT 20 oC (microhm • cm) AT 20 oC (ohm. Circ. Mil/ft) |
118 710 |
|
| MAXIMUM OPERATING TEMPERATURE | 300 oC | 572 oF |
| MELTING POINT | 1370 oC | 2500 oF |
| COEFFICIENT OF EXPANSION | 12.7 µm/m °C (20 - 100°C) |
|
| RW 122 Properties | ||
| DENSITY | 8.28 g/cm3 | |
| ELECTRICAL RESISTIVITY AT 20 oC (microhm • cm) AT 20 oC (ohm. Circ. Mil/ft) |
122 734 |
|
| MAXIMUM OPERATING TEMPERATURE | 300 oC | 572 oF |
| MELTING POINT | 1430 oC | 2600 oF |
| COEFFICIENT OF EXPANSION | 12.6 µm/m °C (20 - 100°C) |
|
| RW 70 Properties | ||
| DENSITY | 8.00 g/cm3 | |
| ELECTRICAL RESISTIVITY AT 20 oC (microhm • cm) AT 20 oC (ohm. Circ. Mil/ft) |
70 421 |
|
| MAXIMUM OPERATING TEMPERATURE | 300 oC | 572 oF |
| MELTING POINT | 1375 oC | 2500 oF |
| COEFFICIENT OF EXPANSION | 17.6 µm/m °C (20 - 100°C) |
|